Автори | L.V. Kozhitov1 , M.F. Bulatov2, V.V. Korovushkin1 , V.G. Kostishin1 , D.G. Muratov1,3, M.N. Shipko1,4, S.G. Emelyanov5, E.V. Yakushko1 |
Афіліація | 1 National University of Science and Technology «MISiS», 4, Leninsky Pr., 119049 Moscow, Russia 2 JSC "State research and design Institute of rare-metal industry "Giredmet", 5-1, G. Tolmachevsky Lane, 119017 Moscow, Russia 3 A.V. Topchiev Institute of Petrochemical Synthesis, RAS, 29, Leninsky Pr., 119991 Moscow, Russia 4 Russian University of Economics named after G. V. Plekhanov, 117997 Moscow, Russia 5 South-West State University, 94, 50 let Oktyabrya St., 305040 Kursk, Russia; |
Е-mail | |
Випуск | Том 7, Рік 2015, Номер 4 |
Дати | Одержано 02.11.2015, опубліковано online - 24.12.2015 |
Цитування | L.V. Kozhitov, M.F. Bulatov, V.V. Korovushkin, et al., J. Nano- Electron. Phys. 7 No 4, 04103 (2015) |
DOI | |
PACS Number(s) | 76.80. + y, 81.05.Mh, 78.67.Bf |
Ключові слова | Mossbauer spectroscopy (3) , Metal-carbon nanocomposites (6) , FeCo Nanoparticles, XRF-analysis, IR-heating (3) . |
Анотація | The features the phase transitions and phase composition of the metal-carbon nanocomposites FeCo / C were studied by Mossbauer spectroscopy. Nanocomposites were synthesized in the temperature range of T = 300-800 °C. It was shown that the samples synthesized at T = 300 °C contains of superparamagnetic nanoparticles of magnetite and amorphous oxide of iron only. The process of forming nanoparticles of alloy FeCo occurs within the temperature range 500-600 ° C due to the recovery of amorphous iron oxide and magnetite as well as them dissolving in a phase of cobalt. The growth of size of nanoparticles of alloy by agglomeration and dissolution of iron in the alloy nanoparticles occurs only at the temperature range of synthesis 600-800 ° C. This is confirmed by a decrease of the content of Fe, which associated with carbon and it is consistent with the results of phase and structural studies, carried out in previous works. |