Автори | V.M. Makarov1 , S.Z. Kalaeva1 , I.N. Zakharova1, I.A. Nevzorov1, M.S. Maltseva1, A.M. Shipilin2 , M.G. Krzhizhanovskaya3 |
Афіліація | 1 Yaroslavl State Technical University, 88, Moskovskij Prosp., 150053 Yaroslavl, Russia 2 M.V. Lomonosov Moscow State University, 1, Leninskiye Gory, 119991 Moscow, Russia 3 Saint-Petersburg State University, 7-9, University Emb., 199034 St. Petersburg, Russia |
Е-mail | |
Випуск | Том 7, Рік 2015, Номер 4 |
Дати | Одержано 28.09.2015, опубліковано online - 10.12.2015 |
Цитування | V.M. Makarov, S.Z. Kalaeva, I.N. Zakharova, et al., J. Nano- Electron. Phys. 7 No 4, 04010 (2015) |
DOI | |
PACS Number(s) | 82.45.Aa. 82.80.Ej |
Ключові слова | Magnetite (6) , Electrocoagulation, Calcination temperature, Powder XRD (2) , Magnetization (18) . |
Анотація | In the current work we discuss the processes occurring along with the temperature treatment of the samples of chromium containing sludge. The results of powder X-ray diffraction and vibrational magnetometry show that magnetite forms in the samples with the increase of the calcination temperature higher than 500 °C. Its quantity increases with the heating, which is clearly visible from the value of saturation magnetization obtained for the samples after various temperature treatments. |